Abstract
The sample is heated under standard conditions to a final temperature of 600 C. The coke residue obtained is classified by reference to a series of standard residues. If the coke residue produced is so swollen that it fills the crosssection of the retort tube, the determination is repeated with the coal admixed with a suitable quantity of electrode carbon or equivalent material.
-
Status: WithdrawnPublication date: 1982-02
-
Edition: 2Number of pages: 9
-