Тезис
Applicable to products having contents of AlF3 of more than 0.15 % (m/m) or of NaF of more than 0.4 % (m/m). Covers sintering of a test portion with a known quantity of sodium fluoride in a muffle furnace at a temperature of (790 10) °C. Under these conditions, aluminium fluoride in excess of that required by the stoichiometric formula AlF3 .3NaF reacts to form cryolite; extraction of the ground sintered mass with boiling water. Acidification with hydrochloric acid solution to a pH less than 3.7 and titration of the excess sodium fluoride with thorium nitrate solution in the presence of alizarin-S as indicator. Has also been approved by the IUPAC.
Общая информация
-
Текущий статус: ОтозваноДата публикации: 1977-11Этап: Отмена международного стандарта [95.99]
-
Версия: 1
-
Технический комитет :ISO/TC 226ICS :71.060.50
- RSS обновления
Жизненный цикл
-
Сейчас
-
00
Предварительная стадия
-
10
Стадия, связанная с внесением предложения
-
20
Подготовительная стадия
-
30
Стадия, связанная с подготовкой проекта комитета
-
40
Стадия, связанная с рассмотрением проекта международного стандарта
-
50
Стадия, на которой осуществляется принятие стандарта
-
60
Стадия, на которой осуществляется публикация
-
90
Стадия пересмотра
-
95
Стадия, на которой осуществляется отмена стандарта
-
00